ASTM B127-19
Standard Specification for Nickel-Copper Alloy Plate, Sheet, and Strip
ASTM B127 ASME SB 127 specification covers rolled nickel-copper alloy (UNS N04400) plate, sheet, and strip. The Monel 400 UNS N04400 material shall conform to the required chemical composition for nickel, copper, iron, manganese, carbon, silicon, and sulfur.
ASTM B127 is the standard specification for the nickel-copper alloy Monel 400 (UNS N04400) plate, sheet, and strip. The Monel 400 material supplied by HT PIPE can be either hot rolled or cold rolled which are further classified by thickness.
Monel ASTM B127 N04400 Plate Sheet Strip Type
| Monel 400 hot-rolled plate | 3/16"(4.76 mm)and over |
| Monel 400 hot-rolled sheet | {{0}}.018" Less than or equal to T Less than or equal to 0.250"[0.46mm Less than or equal to T Less than or equal to 6.4 mm] |
| Monel 400 cold-rolled sheet | {{0}}.018" Less than or equal to T Less than or equal to 0.250"[0.46mm Less than or equal to T Less than or equal to 6.4 mm] |
| Monel 400 cold-rolled strip | {{0}}.005" Less than or equal to T Less than or equal to 0.250"[0.46mm Less than or equal to T Less than or equal to 6.4 mm] |
ASTM B127 UNS N04400 Chemical Composition
| Greater than or equal to 63.0 | |
| 28.0~34.0 | |
| Less than or equal to 2.50 | |
| Less than or equal to 2.00 | |
| Less than or equal to 0.30 | |
| Less than or equal to 0.50 | |
| Less than or equal to 0.24 |
Mechanical Properties of Monel 400 Hot-Rolled Plate
| Elongation in 2", min. % |
|||
| 70 [485] | 28 [195] | 35 | |
| As-Rolled | 75 [515] | 40 [275] | 25 |